Galvanic Corrosion Checks for Mixed-Metal Hardware Assemblies

A metal fitting can look sound as an individual part and still cause trouble after assembly. A steel hook may be joined to a stainless rivet, or a plated buckle may contact an aluminium plate. If dissimilar metals touch in the presence of an electrolyte such as moisture, one metal can corrode faster than it would on its own. AMPP’s galvanic corrosion overview explains the mechanism. The buyer’s task is to examine the complete joint rather than approve each shiny component separately.

Map the contact points

Start with the assembled product drawing or a physical sample. Identify every metal-to-metal contact: fasteners, pins, swivel joints, welded or crimped interfaces and decorative plates. Note whether water can collect in a crevice or remain trapped beneath webbing. A dry indoor accessory and an outdoor leash or equestrian fitting have different exposure profiles, even if their nominal hardware materials are the same.

Ask the supplier to state the base metal and coating of each component, not merely its colour. A specification such as “silver finish” cannot reveal whether a joint combines zinc-plated steel, stainless steel and aluminium. If a coating is intended to separate the metals, inspect how it behaves at cut edges, threads and wear points where contact may return during use.

Treat the assembly as the test article

Isolating washers, sleeves or coatings may reduce direct electrical contact, but they must be compatible with the product’s strength, movement and cleaning requirements. A material substitution can change both corrosion behaviour and mechanical fit. Agree on any proposed change before production, record the approved combination by part number and update the drawing or bill of materials.

When exposure is important, test the assembled configuration under conditions relevant to its use. Examine the joint after the test, not just the visible outer surface. Record the acceptance criteria in advance: staining, red corrosion, seized movement, coating loss or loss of strength may matter differently for different products. A generic salt-spray duration alone does not establish service life.

The Metal Hardware Buyer Guides help connect material, finish and inspection requirements in a sourcing request. One practical RFQ question is: “Which dissimilar metals contact in the finished assembly, and what prevents retained moisture at those joints?”

Source: AMPP, Galvanic Corrosion.